The distribution and degradation of radiolabeled superparamagnetic iron oxide nanoparticles and quantum dots in mice

Standard

The distribution and degradation of radiolabeled superparamagnetic iron oxide nanoparticles and quantum dots in mice. / Bargheer, Denise; Giemsa, Artur; Freund, Barbara; Heine, Markus; Waurisch, Christian; Stachowski, Gordon M; Hickey, Stephen G; Eychmüller, Alexander; Heeren, Jörg; Nielsen, Peter.

In: BEILSTEIN J NANOTECH, Vol. 6, 09.01.2015, p. 111-23.

Research output: SCORING: Contribution to journalSCORING: Journal articleResearchpeer-review

Harvard

Bargheer, D, Giemsa, A, Freund, B, Heine, M, Waurisch, C, Stachowski, GM, Hickey, SG, Eychmüller, A, Heeren, J & Nielsen, P 2015, 'The distribution and degradation of radiolabeled superparamagnetic iron oxide nanoparticles and quantum dots in mice', BEILSTEIN J NANOTECH, vol. 6, pp. 111-23. https://doi.org/10.3762/bjnano.6.11

APA

Bargheer, D., Giemsa, A., Freund, B., Heine, M., Waurisch, C., Stachowski, G. M., Hickey, S. G., Eychmüller, A., Heeren, J., & Nielsen, P. (2015). The distribution and degradation of radiolabeled superparamagnetic iron oxide nanoparticles and quantum dots in mice. BEILSTEIN J NANOTECH, 6, 111-23. https://doi.org/10.3762/bjnano.6.11

Vancouver

Bibtex

@article{20e20e0551e243c8a4687d95f9865b07,
title = "The distribution and degradation of radiolabeled superparamagnetic iron oxide nanoparticles and quantum dots in mice",
abstract = "(51)Cr-labeled, superparamagnetic, iron oxide nanoparticles ((51)Cr-SPIOs) and (65)Zn-labeled CdSe/CdS/ZnS-quantum dots ((65)Zn-Qdots) were prepared using an easy, on demand, exchange-labeling technique and their particokinetic parameters were studied in mice after intravenous injection. The results indicate that the application of these heterologous isotopes can be used to successfully mark the nanoparticles during initial distribution and organ uptake, although the (65)Zn-label appeared not to be fully stable. As the degradation of the nanoparticles takes place, the individual transport mechanisms for the different isotopes must be carefully taken into account. Although this variation in transport paths can bring new insights with regard to the respective trace element homeostasis, it can also limit the relevance of such trace material-based approaches in nanobioscience. By monitoring (51)Cr-SPIOs after oral gavage, the gastrointestinal non-absorption of intact SPIOs in a hydrophilic or lipophilic surrounding was measured in mice with such high sensitivity for the first time. After intravenous injection, polymer-coated, (65)Zn-Qdots were mainly taken up by the liver and spleen, which was different from that of ionic (65)ZnCl2. Following the label for 4 weeks, an indication of substantial degradation of the nanoparticles and the release of the label into the Zn pool was observed. Confocal microscopy of rat liver cryosections (prepared 2 h after intravenous injection of polymer-coated Qdots) revealed a colocalization with markers for Kupffer cells and liver sinusoidal endothelial cells (LSEC), but not with hepatocytes. In J774 macrophages, fluorescent Qdots were found colocalized with lysosomal markers. After 24 h, no signs of degradation could be detected. However, after 12 weeks, no fluorescent nanoparticles could be detected in the liver cryosections, which would confirm our (65)Zn data showing a substantial degradation of the polymer-coated CdSe/CdS/ZnS-Qdots in the liver.",
author = "Denise Bargheer and Artur Giemsa and Barbara Freund and Markus Heine and Christian Waurisch and Stachowski, {Gordon M} and Hickey, {Stephen G} and Alexander Eychm{\"u}ller and J{\"o}rg Heeren and Peter Nielsen",
year = "2015",
month = jan,
day = "9",
doi = "10.3762/bjnano.6.11",
language = "English",
volume = "6",
pages = "111--23",
journal = "BEILSTEIN J NANOTECH",
issn = "2190-4286",
publisher = "Beilstein-Institut Zur Forderung der Chemischen Wissenschaften",

}

RIS

TY - JOUR

T1 - The distribution and degradation of radiolabeled superparamagnetic iron oxide nanoparticles and quantum dots in mice

AU - Bargheer, Denise

AU - Giemsa, Artur

AU - Freund, Barbara

AU - Heine, Markus

AU - Waurisch, Christian

AU - Stachowski, Gordon M

AU - Hickey, Stephen G

AU - Eychmüller, Alexander

AU - Heeren, Jörg

AU - Nielsen, Peter

PY - 2015/1/9

Y1 - 2015/1/9

N2 - (51)Cr-labeled, superparamagnetic, iron oxide nanoparticles ((51)Cr-SPIOs) and (65)Zn-labeled CdSe/CdS/ZnS-quantum dots ((65)Zn-Qdots) were prepared using an easy, on demand, exchange-labeling technique and their particokinetic parameters were studied in mice after intravenous injection. The results indicate that the application of these heterologous isotopes can be used to successfully mark the nanoparticles during initial distribution and organ uptake, although the (65)Zn-label appeared not to be fully stable. As the degradation of the nanoparticles takes place, the individual transport mechanisms for the different isotopes must be carefully taken into account. Although this variation in transport paths can bring new insights with regard to the respective trace element homeostasis, it can also limit the relevance of such trace material-based approaches in nanobioscience. By monitoring (51)Cr-SPIOs after oral gavage, the gastrointestinal non-absorption of intact SPIOs in a hydrophilic or lipophilic surrounding was measured in mice with such high sensitivity for the first time. After intravenous injection, polymer-coated, (65)Zn-Qdots were mainly taken up by the liver and spleen, which was different from that of ionic (65)ZnCl2. Following the label for 4 weeks, an indication of substantial degradation of the nanoparticles and the release of the label into the Zn pool was observed. Confocal microscopy of rat liver cryosections (prepared 2 h after intravenous injection of polymer-coated Qdots) revealed a colocalization with markers for Kupffer cells and liver sinusoidal endothelial cells (LSEC), but not with hepatocytes. In J774 macrophages, fluorescent Qdots were found colocalized with lysosomal markers. After 24 h, no signs of degradation could be detected. However, after 12 weeks, no fluorescent nanoparticles could be detected in the liver cryosections, which would confirm our (65)Zn data showing a substantial degradation of the polymer-coated CdSe/CdS/ZnS-Qdots in the liver.

AB - (51)Cr-labeled, superparamagnetic, iron oxide nanoparticles ((51)Cr-SPIOs) and (65)Zn-labeled CdSe/CdS/ZnS-quantum dots ((65)Zn-Qdots) were prepared using an easy, on demand, exchange-labeling technique and their particokinetic parameters were studied in mice after intravenous injection. The results indicate that the application of these heterologous isotopes can be used to successfully mark the nanoparticles during initial distribution and organ uptake, although the (65)Zn-label appeared not to be fully stable. As the degradation of the nanoparticles takes place, the individual transport mechanisms for the different isotopes must be carefully taken into account. Although this variation in transport paths can bring new insights with regard to the respective trace element homeostasis, it can also limit the relevance of such trace material-based approaches in nanobioscience. By monitoring (51)Cr-SPIOs after oral gavage, the gastrointestinal non-absorption of intact SPIOs in a hydrophilic or lipophilic surrounding was measured in mice with such high sensitivity for the first time. After intravenous injection, polymer-coated, (65)Zn-Qdots were mainly taken up by the liver and spleen, which was different from that of ionic (65)ZnCl2. Following the label for 4 weeks, an indication of substantial degradation of the nanoparticles and the release of the label into the Zn pool was observed. Confocal microscopy of rat liver cryosections (prepared 2 h after intravenous injection of polymer-coated Qdots) revealed a colocalization with markers for Kupffer cells and liver sinusoidal endothelial cells (LSEC), but not with hepatocytes. In J774 macrophages, fluorescent Qdots were found colocalized with lysosomal markers. After 24 h, no signs of degradation could be detected. However, after 12 weeks, no fluorescent nanoparticles could be detected in the liver cryosections, which would confirm our (65)Zn data showing a substantial degradation of the polymer-coated CdSe/CdS/ZnS-Qdots in the liver.

U2 - 10.3762/bjnano.6.11

DO - 10.3762/bjnano.6.11

M3 - SCORING: Journal article

C2 - 25671156

VL - 6

SP - 111

EP - 123

JO - BEILSTEIN J NANOTECH

JF - BEILSTEIN J NANOTECH

SN - 2190-4286

ER -