Plasma arc curing of ceramic brackets: an evaluation of shear bond strength and debonding characteristics.

Related Research units

Abstract

The aim of this in vitro investigation was to evaluate bond strength and debonding characteristics when a xenon plasma arc curing light is used to bond polycrystalline and monocrystalline ceramic brackets. Brackets were bonded to 240 extracted bovine mandibular incisors with a composite adhesive. Curing intervals of 1, 3, and 6 seconds were chosen for curing with the plasma arc light, and the control group was cured at 10 seconds per bracket with a conventional halogen light. Debonding was performed on a universal testing machine and according to the bracket manufacturers' recommendations. Both the polycrystalline and the monocrystalline brackets consistently debonded at the bracket-adhesive interface, regardless of debonding method, curing interval, or curing light. No enamel fractures were observed after debonding. Bracket fractures were rare and did not affect debonding. Bond strength was significantly higher for the monocrystalline brackets (P

Bibliographical data

Original languageGerman
Article number3
ISSN0889-5406
Publication statusPublished - 2003
pubmed 12970665